Resolution: standard / high Figure 3.
Device performance of the devices made by spin-coating or electrospraying. The thicknesses of EML were as follows: (1) 78, (2) 100, (3) 120, (4) 70, (5) 100,
and (6) 103 nm.
Hwang et al. Nanoscale Research Letters 2012 7:52 doi:10.1186/1556-276X-7-52 |