Figure 4.

Raman back scattering spectra of nonirradiated and irradiated CdZnTe sample. Intensities of LR are as follows: I = 0, black curve; I = 2.8 MW/cm2, blue curve; I = 8.6 MW/cm2, green curve; and I = 11.0 MW/cm2, red curve.

Medvid' et al. Nanoscale Research Letters 2012 7:514   doi:10.1186/1556-276X-7-514