Resolution: standard / high Figure 1.
Atomic force microscope 3D image of the Cd1âxZnxTe (xâ=â0.1) surfaces after irradiation by the laser at intensity of 12âMW/cm2. The blue and red curly arrows show the different surfaces with different luminescence
properties.
Medvid' et al. Nanoscale Research Letters 2012 7:514 doi:10.1186/1556-276X-7-514 |