Figure 6.
PL spectra of an about 3.4-μm diameter porous silicon colloid. After being immersed in 200-mM NADPH aqueous solution during 1 (bottom spectrum)
and 5 h (top spectrum).
Ramiro-Manzano et al. Nanoscale Research Letters 2012 7:497 doi:10.1186/1556-276X-7-497 |