Figure 4.

X-ray diffraction patterns of sintered ceramics. X-ray diffraction patterns of the 0, 0.1, 0.15, and 0.2 wt.% Y2O3-doped AZO ceramics sintered at 1,300°C.

Yang et al. Nanoscale Research Letters 2012 7:481   doi:10.1186/1556-276X-7-481