Table 1 |
|||||
| Pore fabrication conditions for PbTe films | |||||
| Sample number | ja(mA·cm−2) | ta(min) | d(nm) | dpor(nm) | Porosity (%) |
| 1 | 2 | 10 | 510 | 180 | 41 |
| 2 | 2 | 20 | 790 | 160 | 52 |
| 3 | 4 | 18 | 440 | 140 | 52 |
ja, anodizing current density; ta, anodizing time; d, thickness; dpor, thickness of the porous layer.
Zimin et al. Nanoscale Research Letters 2012 7:442 doi:10.1186/1556-276X-7-442