Figure 4.

Dependence of residual strain on sin2ψ for 200-nm-thick BFO films. The films were grown on (a) 20- and (b) 30-nm-thick L10-FePt bottom electrodes at a Td of 400 °C.

Chang et al. Nanoscale Research Letters 2012 7:435   doi:10.1186/1556-276X-7-435