Resolution: standard / high Figure 6.
Relationship between P-E hysteresis loops and MoO3 content of Bi3.25La0.75(Ti1-xMox)3O12 ceramics. The measurement was done at a frequency of 50 Hz for BLTM ceramics sintered at 1,100°C.
Siriprapa et al. Nanoscale Research Letters 2012 7:42 doi:10.1186/1556-276X-7-42 |