Figure 4.

Result of element analysis by EDX for (A) untreated PSi and (B) treated with 6.0-μM RC. The corresponding elements found in the samples are also indicated.

Hajdu et al. Nanoscale Research Letters 2012 7:400   doi:10.1186/1556-276X-7-400