Resolution: standard / high Figure 3.
Change in T-NT diameter with anodization potential after 1 h anodization. The gap between electrodes was 2 cm. Insets show SEM micrographs of T-NT formed by
anodization at 10, 30, and 50 V.
Chappanda et al. Nanoscale Research Letters 2012 7:388 doi:10.1186/1556-276X-7-388 |