Figure 3.

FTIR spectra of PMHS polysiloxanes reacted with VCHE at different stages. (a) Pure PMHS precursor; (b) reacted at 35°C for 24 h; (c) reacted at 35°C for 24 h and then at 80°C for 24 h.

Zhang et al. Nanoscale Research Letters 2012 7:380   doi:10.1186/1556-276X-7-380
Download authors' original image