Table 1

Geometric characteristics of the NAA samples (interpore distance (dint) and porosity (P) -*P= Π/(2√3))·(dp/dint)2)
Label Lp(μm) dp(nm) dint(nm) P (%)*
R-OSC(1) 5.0 ± 0.1 30 ± 3 103 ± 4 8.2 ± 1.7
R-OSC(2) 5.0 ± 0.1 41 ± 3 103 ± 4 15.2 ± 2.7
R-OSC(3) 5.0 ± 0.1 52 ± 3 103 ± 4 24.5 ± 4.2
R-OSC(4) 5.0 ± 0.1 71 ± 2 103 ± 4 44.4 ± 5.5
R-OSC(5) 5.0 ± 0.1 30 ± 3 103 ± 4 8.2 ± 1.7
R-OSC(6) 8.7 ± 0.1 30 ± 3 103 ± 4 8.2 ± 1.7
R-OSC(7) 12.4 ± 0.2 30 ± 3 103 ± 4 8.2 ± 1.7