Figure 8.

3D view using optical profilometry of a sample surface etched during 45 s at 20 mA. The limit between the exposed area where the polishing defects are revealed and the protected one is clearly visible.

Gautier et al. Nanoscale Research Letters 2012 7:367   doi:10.1186/1556-276X-7-367