Resolution: standard / high Figure 3.
Measured potential during the initiation of the pores. The initiation was carried out for a fixed current density of 25.5 mA/cm2 in the case of SiC (C and Si faces). Two samples were etched using the same conditions.
As a comparison, the curve for a highly doped silicon wafer is also shown. The samples
#1, #2 and #3, #4 are identical.
Gautier et al. Nanoscale Research Letters 2012 7:367 doi:10.1186/1556-276X-7-367 |