Figure 1.

Cyclic voltammograms of TiO2nt electrode. In (a) 0.035 M LiTFSI and (b) in 0.035 M LiTFSI + 4 g MMA-PEO at the 1st, 3rd, 5th, and 10th cycles. The electropolymerization was carried out between −0.4 and −2.5 V vs Hg/Hg2SO4, K2SO4 (saturated) with the scan rate of 25 mV/s.

Plylahan et al. Nanoscale Research Letters 2012 7:349   doi:10.1186/1556-276X-7-349