Resolution: standard / high Figure 3.
Recorded differential-pulsed voltammograms (0.2 V modulation amplitude, 0.02 V step
potential). They were recorded at (a) AgCNF, (b) AgZCNF electrodes in 0.1 M Na2SO4 supporting electrolyte and in the presence of various IBP concentrations that consists
0.5 to 5 mg.Lā1 (curves 2 to 11). Inset: calibration plots of the anodic current recorded at Eā=ā+1.15
V vs. IBP concentration.
Manea et al. Nanoscale Research Letters 2012 7:331 doi:10.1186/1556-276X-7-331 |