Table 2 |
||||
|
Sun-Voc parameters of the processed solar cells with different Mg thicknesses without an oxidation step |
||||
|
Sample |
Voc (mV) |
Jsc (mA/cm2) |
FF (%) |
EFF (%) |
|
|
||||
|
Mg200 Å |
602 |
36.9 |
80.1 |
17.75 |
|
Mg300 Å |
598 |
36 |
78.6 |
16.99 |
|
Mg400 Å |
600 |
35 |
78.4 |
16.67 |
|
|
||||
|
Voc, open-circuit voltage; Jsc, short-circuit current density; FF, fill factor; EFF, efficiency. |
||||
|
Lee et al. Nanoscale Research Letters 2012 7:32 doi:10.1186/1556-276X-7-32 |
||||