Table 2 |
|||
| Electrical behavior of multilayer ZnO/Ag/ZnO samples manufactured with or without IAD | |||
|
Average transmittance (400–700 nm) |
sheet resistance (ohm/sq) |
Crystallinity of the metal layer |
|
|
Glass substrate With IAD |
93% | 5.08 | Polycrystalline |
|
Glass substrate Without IAD |
68% | 10.51 | Amorphous |
|
Plastic substrate With IAD |
81% | 6.03 | Polycrystalline |
|
Plastic substrate Without IAD |
46% | 13.2 | Amorphous |
Chiu et al. Nanoscale Research Letters 2012 7:304 doi:10.1186/1556-276X-7-304