Figure 1.

Alloy quenched after a solution treatment at 430°C for 24 h. The incident electron beam was parallel to <a onClick="popup('','MathML',630,470);return false;" target="_blank" href="">View MathML</a>. (a) HAADF image, (b) Zr EDXS map, (c) Zn EDXS map and (d) a combined EDXS map of Zr and Zn.

Zhu et al. Nanoscale Research Letters 2012 7:300   doi:10.1186/1556-276X-7-300