Figure 2.

Sheet resistances of the hybrid electrodes with 0 to 50 wt.% of SWCNTs. The transparency of the hybrid electrodes is constant (80%). Hybrid electrodes were fabricated by low-temperature processing at 60°C.

Tokuno et al. Nanoscale Research Letters 2012 7:281   doi:10.1186/1556-276X-7-281