Figure 3.

SEM images of Cu2O samples obtained with different concentrations of EDA. The concentrations of NaOH solution is 15 mol L−1 and the concentrations of EDA were as follows: (a) 0 μL (EDA)/28 mL (total solution) (SI1-B1 in Additional file 1), (b) 70 μL/28 mL (SI1-B2 in Additional file 1), (c) 150 μL/28 mL (SI1-B3 in Additional file 1), and (d) 300 μL/28 mL (SI1-B4 in Additional file 1). The inset is the corresponding TEM morphology of the Cu2O crystal.

Feng et al. Nanoscale Research Letters 2012 7:276   doi:10.1186/1556-276X-7-276