Figure 6.

Temperature dependence of the yellow-orange emission peak energy. For the indium-doped ZnO nanostructures after annealing at different temperatures.

Wang et al. Nanoscale Research Letters 2012 7:270   doi:10.1186/1556-276X-7-270