Figure 2.

XRD patterns of BNKT-BST ceramics. The samples were sintered at 1,125°C. (a) 2θ = 10° to 80° and (b) 2θ = 44° to 48°.

Jaita et al. Nanoscale Research Letters 2012 7:24   doi:10.1186/1556-276X-7-24