Figure 2.

XRD patterns of Ti-6Al-4V alloys. Nitriding at 850°C for (a) 1, (b) 6, and (c) 12 h.

Lee et al. Nanoscale Research Letters 2012 7:21   doi:10.1186/1556-276X-7-21