Resolution: standard / high Figure 1.
Film-to-fiber processing. (a) Freestanding SWNT thin film with a coin on it. (b) Fiber formation through a wetting/drying process. (c) Fiber twisting. (d) A single fiber bearing a 200-g weight.
Jia et al. Nanoscale Research Letters 2012 7:137 doi:10.1186/1556-276X-7-137 |