Figure 5.

Time dependence of the emission current of the in situ-grown SnO2 nanowire arrays. The characterization was measured at a fixed applied voltage (500 V) with an anode-cathode separation of 100 μm.

Zhou et al. Nanoscale Research Letters 2012 7:117   doi:10.1186/1556-276X-7-117