Figure 2.

XRD patterns of Li4Ti5O12 powders. Li4Ti5O12 prepared through wet and solid-state processes and subsequently calcined at 700°C and 800°C for 4 h. (By Jin YH et al.).

Jin et al. Nanoscale Research Letters 2012 7:10   doi:10.1186/1556-276X-7-10