Resolution: standard / high Figure 4.
AFM (a, b, c, e) and STEM (d, f) images of CdTe quantum dots. a–c AFM images of quantum dots dispersed on mica (dispersed from aqueous solution kept
for: a 40 min, b 5 h, c 24 h), d STEM image of quantum dots dispersed on TEM grid (dispersed from solution kept for
48 h), e AFM image of quantum dots with BSA dispersed on mica (dispersed from aqueous solution
kept for 2 months), f STEM image of quantum dots with BSA (dispersed from aqueous solution kept for 2 months).
Inserts (in d and f images) show magnified view (40 nm × 40 nm). Concentrations of solutions used for
sample preparation were 6 × 10-6 mol/l.
Poderys et al. Nanoscale Res Lett 2011 6:9 doi:10.1007/s11671-010-9740-9 |