Resolution: standard / high Figure 3.
SEM images and EDS spectra for Ag NW, respectively, before coating (a) (d), after
coating (b) (e), and after intensive HCl treatment (c) (f).
Liu and Yu Nanoscale Research Letters 2011 6:75 doi:10.1186/1556-276X-6-75 |