Table 1 |
||||
|
Effect of silane-coating thickness of CNFs on permittivity of the nanocomposites before and after wear testing |
||||
|
Samples |
Thickness of silane coating on CNF surface (nm) |
Permittivity before wearing |
Permittivity after 120-h wearing |
Slope (from Fig. 4) × 10-3 |
|
|
||||
|
Nanocomp-ox |
0 |
5.2 |
6.3 |
8.75 |
|
Nanocomp-A |
1.2 |
4.8 |
5.3 |
3.96 |
|
Nanocomp-B |
2.8 |
4.6 |
4.9 |
3.88 |
|
Nanocomp-C |
46 |
4.1 |
4.4 |
1.51 |
|
|
||||
|
Liu et al. Nanoscale Res Lett 2011 6:7 doi:10.1007/s11671-010-9748-1 |
||||