Table 1 |
||
|
Hybrid milling conditions used for SPPC fabrication |
||
|
Structure |
30-kV mill time (s) |
5-kV mill time (s) |
|
|
||
|
A |
5 |
N/A |
|
B |
5 |
Image only |
|
C |
3 |
22 |
|
D |
3 |
45 |
|
E |
4 |
45 |
|
|
||
|
Einsle et al. Nanoscale Research Letters 2011 6:572 doi:10.1186/1556-276X-6-572 |
||