Relationships between film thickness, grain diameter, and deposition time. At a source temperature at or above 420°C, the ZnO film thickness scales linearly with deposition time at a growth rate of 16.7 nm/min. Grain diameter also increases as deposition duration increases.

Pedersen et al. Nanoscale Research Letters 2011 6:568   doi:10.1186/1556-276X-6-568