Resolution: standard / high Figure 4.
Current images of SnO2 nanobelt. (a) Surface topography, (b) current maps at -4.0 V, (c) reduced current images in the second scan at -4.0 V.
Wang et al. Nanoscale Research Letters 2011 6:541 doi:10.1186/1556-276X-6-541 |