Figure 1.

XRD patterns of the initial Ti33Cu67 ribbon and ribbons crystallized under different electrical pulse conditions. (see Table 1).

Dudina et al. Nanoscale Research Letters 2011 6:512   doi:10.1186/1556-276X-6-512