Table 1 |
||
|
FoM calculated for several types of high dielectric constant filler/silicone composites |
||
|
Filler |
Filler loading (wt.%) |
FoM |
|
|
||
|
TiO2 [3] |
70.0 |
3.33 (at 1 Hz) |
|
TiO2 [4] |
30.0 |
1.11 (at 10 Hz) |
|
PMN-PT [3] |
70.0 |
2.38 (at 1 Hz) |
|
BaTiO3 [3] |
70.0 |
8.09 (at 1 Hz) |
|
PHT [20] |
1.0 |
21.42 (at 10 Hz) |
|
CuPc [21] |
20.0 |
5.0 (at 1 kHz) |
|
CNT* |
0.5 |
14.8 (at 10 Hz) |
|
FGS* |
0.5 |
157.77 (at 10 Hz) |
|
FGS* |
2.0 |
366.29 (at 10 Hz) |
|
|
||
|
*Values reported in the present work |
||
|
Romasanta et al. Nanoscale Research Letters 2011 6:508 doi:10.1186/1556-276X-6-508 |
||