Resolution: standard / high Figure 3.
SEM image of InP. After 2 h of electrophoretic deposition of Pd NPs (right side) and graphite Schottky
contact (left side). The scale 1 μm is shown with the bright bar at the bottom of
the image.
Zdansky Nanoscale Research Letters 2011 6:490 doi:10.1186/1556-276X-6-490 |