Figure 1.

X-ray diffraction data for La0.35Zr0.65O2 films deposited by ALD and then annealed in air or N2 for 15 min at different temperatures.

Zhao et al. Nanoscale Res Lett 2011 6:48   doi:10.1007/s11671-010-9782-z