Table 1 |
|||||
|
Summary of the deposition conditions and electrical characteristics of the samples prepared on methanol-treated substrates |
|||||
|
Sample |
Time (h) |
Voltage (V) |
R at 1.5 V |
ϕb (eV) |
S at 0.1%H2 |
|
|
|||||
|
InP-Pd-27 |
0.5 |
100 |
1.8E7 |
0.93 |
5.0E4 |
|
InP-Pd-21 |
1 |
100 |
4.8E7 |
0.95 |
4.8E5 |
|
InP-Pd-22 |
2 |
100 |
0.7E7 |
0.88 |
1.6E4 |
|
InP-Pd-09 |
18 |
100 |
1.0E4 |
0.74 |
4.9E2 |
|
|
|||||
|
R is the rectification ratio, ϕb is the Schottky barrier height, and S is the sensing response |
|||||
|
Grym et al. Nanoscale Research Letters 2011 6:392 doi:10.1186/1556-276X-6-392 |
|||||