Figure 3.

Temperature-dependent PL spectra: for sample (a) #987 implanted with 1 × 1015 atoms.cm-2 and annealed at 1100°C and (b) #989 implanted with 1 × 1013 atoms.cm-2 and annealed at 1000°C obtained with 4.7 eV excitation.

Peres et al. Nanoscale Research Letters 2011 6:378   doi:10.1186/1556-276X-6-378