Resolution: standard / high Figure 7.
Normalized photoluminescence spectra of ZnO nanorod layers deposited using different
solvents. The layers are deposited onto ITO/SGL substrate at 480°C from aqueous or alcoholic
solution, illustrated by spectrum A and B, respectively. Spray rate is kept similar
(2.2 ml/min). Spectrum A is shown with fitting results. SEM image of the sample corresponding
to spectrum B is presented in Figure 3c.
Kärber et al. Nanoscale Research Letters 2011 6:359 doi:10.1186/1556-276X-6-359 |