Resolution: standard / high Figure 4.
Photoluminescence spectra at 10 K of the spray pyrolysis-deposited ZnO nanorod layers. The layers were deposited from aqueous solution onto SGL or ITO/SGL substrates,
illustrated by spectrum A and B, respectively. The growth temperature (550°C) and
spray rate (6.2 ml/min) were kept similar. The inset shows the photoluminescence spectrum
at 300 K in region of 2.0-3.4 eV, characteristic of ZnO nanorods deposited onto ITO/SGL
substrate at temperature of 550°C.
Kärber et al. Nanoscale Research Letters 2011 6:359 doi:10.1186/1556-276X-6-359 |