Figure 4.

Cracking density as a function of the substrate nominal strain for different GZO coatings deposited on PEN (82 μm) and the crack density evolution of the PEN/GZO coatings.

Samantilleke et al. Nanoscale Research Letters 2011 6:309   doi:10.1186/1556-276X-6-309