Table 2

Critical buckling force (F), pressure (P), and strain (ε) of pristine (P) SWCNTs and SWCNTs with Stone–Wales (SW) and single vacancy (SV) defects

FP (nN)

PP (GPa)

εp

FSW(nN)

PSW(GPa)

εSW

FSV(nN)

PSV(GPa)

εSV


(3,3)

0.740

8.644

0.477

0.376

4.392

0.102

0.309

3.614

0.083

(4,4)

1.048

9.239

0.718

0.452

3.981

0.129

0.491

4.325

0.157

(5,5)

0.864

6.112

0.488

0.786

5.560

0.453

0.535

3.785

0.187

(6,6)

1.003

5.924

0.658

0.942

5.562

0.625

0.552

3.258

0.199

(3,0)

0.329

6.522

0.135

0.256

5.086

0.105

0.226

4.478

0.063

(4,0)

0.365

5.513

0.167

0.162

2.439

0.042

0.273

4.124

0.093

(5,0)

0.329

3.999

0.136

0.248

3.016

0.099

0.279

3.389

0.097

(6,0)

0.365

3.715

0.167

0.176

1.786

0.049

0.289

2.949

0.106


Ranjbartoreh and Wang Nanoscale Res Lett 2011 6:28   doi:10.1007/s11671-010-9776-x

Open Data