Table 1 |
|||||
|
Effect of Solutol HS15 content on the properties of the copolymer and polymeric micelle at 25°C. |
|||||
|
Mole ratio of mPEG-PLA to Solutol HS 15 |
3:0 |
3:1 |
1:1 |
1:3 |
0:3 |
|
|
|||||
|
CMC (mg/L) |
5.1 |
7.6 |
11.5 |
13.9 |
29.1 |
|
|
|||||
|
Li et al. Nanoscale Research Letters 2011 6:275 doi:10.1186/1556-276X-6-275 |
|||||