Resolution: standard / high Figure 6.
Examples of SEM images of dried samples. The representative photographs were selected for each tested sample. In contrast
to the samples (a, b), the samples (c, d) contain a major part of the nanopowder in the form of fine particles. In addition,
the long-time ultrasonification, see sample (d), breaks-up the remaining clusters apparent in sample (c). The specification of A3 nanopowder is given in Table 1.
Penkavova et al. Nanoscale Research Letters 2011 6:273 doi:10.1186/1556-276X-6-273 |