Resolution: standard / high Figure 6.
Average surface potential obtained by KFM on PPy-diamond, H-diamond, and diamond after
PPy removal. The potential values are referenced to the grounded Au contact pad.
Rezek et al. Nanoscale Research Letters 2011 6:238 doi:10.1186/1556-276X-6-238 |