Figure 6.

Average surface potential obtained by KFM on PPy-diamond, H-diamond, and diamond after PPy removal. The potential values are referenced to the grounded Au contact pad.

Rezek et al. Nanoscale Research Letters 2011 6:238   doi:10.1186/1556-276X-6-238
Download authors' original image