Resolution: standard / high Figure 2.
XRD diffraction patterns of the Fe3O4@PPy deposits prepared under different amounts of pyrrole monomer at 160°C: (a) 0.1 mL, (b) 0.3 mL, (c) 0.5 mL.
Zhao and Nan Nanoscale Research Letters 2011 6:230 doi:10.1186/1556-276X-6-230 |