Figure 4.

The experimental data and the fitted curves from Mn PL transients. Two ZnS/Mn wire samples with a Mn concentration 2.8·10-3 at.% which were implanted at temperatures of 400°C and 600°C, respectively.

Kaiser et al. Nanoscale Research Letters 2011 6:228   doi:10.1186/1556-276X-6-228