Table 2

Summary of experimental parameters

Capacitance

7.5 μF, 30 μF

Charging voltage

3 kV

Material

Silver

Wire diameter

0.1 mm

Wire length

2.8 mm, 3.8 mm

Liquid

Deionized water, Ethanol

Liquid volume

500 mL, 1,000 mL

Ag concentration

0.001 vol.%


Ju Park et al. Nanoscale Research Letters 2011 6:223   doi:10.1186/1556-276X-6-223